MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical strength..

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccapproximately
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68Formulation Example
Tensile Strength 4205 psiFormulation Example
Elongation at Break 310 %Formulation Example
100% Modulus 0.551 ksi
@Strain 100 %
Formulation Example
200% Modulus 1.785 ksi
@Strain 200 %
300% Modulus 3.985 ksi
@Strain 300 %
Formulation Example
Tear Strength 37.0 kN/mFormulation Example
Compression Set 11 %
@Temperature 100 °C,
Time 79200 sec
Formulation Example
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Monthunder dry and cool conditions
 
Descriptive Properties
AppearanceWhite to amber solid bale or milled sheets
Formulation as Tested0.25Stearic Acid
 1TAC
 100Millathane 66
 20N330 Black
 3StabaxolP
 6.5Di-Cup 40 C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mearthane Durethane™ C 10-30A Polyurethane
ATG s.r.l. AU-EU Polyurethane Rubber
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

PMILL010 / 87054

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.