MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 230 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Impact Grade

Material Notes: 30% glass fiber, highest impact resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Moisture Absorption at Equilibrium 1.8 %50% RH; ISO 62
Water Absorption at Saturation 6.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm150x105x3; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 165 MPaISO 2093-1
Tensile Strength at Break 140 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 4.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 8300 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 230 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 210 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 7500 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 5.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 100 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact, Notched 20.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 213 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 190 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1,-2
Vicat Softening Point 200 °C
@Load 5.10 kg
120°C/h; ISO 306
 200 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.40 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD 0.165 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 2577
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °C
Mold Temperature 80.0 °C
Back Pressure 40.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry

PLANW9546 / 208179

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.