MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced engineering thermoplastics in numerous applications.

    Product Features:
  • Good flexural strength
  • Meets or exceeds GMP.PP.017 sepcifications
  • Appearance: Black

    Forms: Pellets

    Processing Method: Injection Moulding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 - 1.15 g/ccASTM D792
Melt Flow 8.0 - 15 g/10 minASTM D1238
Ash 28 - 32 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 8000 psiASTM D638
Flexural Modulus >= 600300 psi
Izod Impact, Notched >= 1.80 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 1239H Glass Filled Chemically Coupled Homopolymer Polypropylene
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled
Overview of materials for Polypropylene with 30% Glass Fiber Filler

PBUCK013 / 104481

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.