MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC/ABS 7700 SK PC/ABS, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Product Description: EMERGE™ PC/ABS 7700 SK advanced resin is an ignition-resistant PC/ABS blends that contains no chlorinated or brominated flame retardant additives. This grade has been tested to ISO 10993 Parts 5 & 10 and is suitable for skin contact applications. It has superior processability for injection molding applications. This grade has excellent aesthetics, is UV stabilized and is available in custom colors.
Main Characteristics: Tested under ISO 10993 (Parts 5 & 10); UV stabilized; RoHS compliant
Applications: Medical equipment housings; Consumer Electronics; Wearable devices

Availability: Asia Pacific; Europe; North America

Additive: UV Stabilizer

Features: Bromine Free; Chlorine Free; Flame Retardant; Good Processability; High Impact Resistance; Ignition Resistant; Pleasing Surface Appearance; UV Stabilized

Uses: Electrical Housing; Electrical/Electronic Applications; Housings; Medical Devices; Medical/Healthcare Applications

Agency Ratings: ISO 10993 Part 10; ISO 10993 Part 5

RoSH Compliance: RoSH Compliant

Appearance: Colors Available

Form: Pellets

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmASTM D955
Melt Flow 11 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 20 g/10 min
@Load 5.00 kg,
Temperature 240 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 6530 psiISO 527-2/50
 7000 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 7980 psiISO 527-2/50
 8700 psi2.0 in/min; ASTM D638
Elongation at Break 43 %ISO 527-2/50
 65 %2.0 in/min; ASTM D638
Elongation at Yield 3.8 %2.0 in/min; ASTM D638
 3.8 %ISO 527-2/50
Tensile Modulus 363000 psiISO 527-1/1
 380000 psi0.039 in/min; ASTM D638
Flexural Strength 14000 psiASTM D790
Flexural Modulus 390000 psiASTM D790
Izod Impact, Notched 3.70 ft-lb/in
@Temperature -17.8 °C
ASTM D256
 8.20 ft-lb/in
@Temperature -6.67 °C
ASTM D256
 9.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 6.70 ft-lb/in²
@Temperature -30.0 °C
ISO 180/1A
 24.0 ft-lb/in²
@Temperature 22.8 °C
ISO 180/1A
Charpy Impact, Notched 7.10 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 19.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmIEC 60093
Surface Resistance 5.20e+15 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.86
@Frequency 100 Hz
IEC 60250
Dielectric Strength 460 V/mil
@Thickness 3.20 mm
in Oil; IEC 60243-1
 660 V/mil
@Thickness 1.60 mm
in Oil; IEC 60243-1
Dissipation Factor 0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 38.0 µin/in-°F
@Temperature -40.0 - 40.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 190 °FAnnealed; ISO 75-2/B
 195 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 171 °FUnannealed; ISO 75-2/A
 175 °FUnannealed; ASTM D648
Vicat Softening Point 201 °FISO 306/B50
 219 °FISO 306/A120
 220 °FRate B (120°C/h), Loading 1 (10 N); ASTM D1525
Flammability, UL94 V-0
@Thickness 1.52 mm
 5VB
@Thickness 2.03 mm
 5VA
@Thickness 2.54 mm
Oxygen Index 28 %ASTM D2863
Glow Wire Ignition Temperature 1290 °F
@Thickness 1.52 mm
IEC 60695-2-13
 1290 °F
@Thickness 2.03 mm
IEC 60695-2-13
 1290 °F
@Thickness 3.05 mm
IEC 60695-2-13
Glow Wire Flammability Index 1700 °F
@Thickness 1.52 mm
IEC 60695-2-12
 1700 °F
@Thickness 2.03 mm
IEC 60695-2-12
 1700 °F
@Thickness 2.54 mm
IEC 60695-2-12
 1740 °F
@Thickness 3.05 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 455 - 527 °F
Mold Temperature 140 - 194 °F
Drying Temperature 176 - 194 °F
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1532 / 312225

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.