MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemours Krytox™ 143AZ PFPE Aerospace Grade Fluorinated Oil
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Many grades and special formulations of Krytox™ oils and greases offer superior performance characteristics and certifications for aerospace applications. They operate effectively in high vacuum and extreme temperatures, and are able to endure exposure to fuels, oxidizers, and radiation.

Features:

  • Unaffected lubricity and viscosity within a wide temperature range
  • Stable physical properties over time, including radiation resistance
  • Virtually unaffected by harsh environments and caustic chemicals
  • Resistant to vapor loss in a vacuum (e.g., during high-altitude orbit or deep space flight)
  • Long wear and low-energy consumption due to excellent friction-reducing characteristics
  • Compatible for use with most metals, elastomers, plastics, paints, and finishes,
  • Nontoxic, nonflammable, inert, and non-evaporative.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.72 g/cc
@Temperature 100 °C
oil
 1.91 g/cc
@Temperature 0.000 °C
oil
Volatiles 18 %
@Treatment Temp. 149 °C,
Time 79200 sec
wt% loss; ASTM D2595
Viscosity Measurement 60Viscosity Index; ASTM D2270
Viscosity Measure 1.1 cSt
@Temperature 204 °C
ASTM D445
 4.1 cSt
@Temperature 100 °C
ASTM D445
 4.2 cSt
@Temperature 99.0 °C
ASTM D445
 22.8 cSt
@Temperature 40.0 °C
ASTM D445
 24.7 cSt
@Temperature 38.0 °C
ASTM D445
 60 cSt
@Temperature 20.0 °C
ASTM D445
 228 cSt
@Temperature 0.000 °C
ASTM D445
 7480 cSt
@Temperature -32.0 °C
ASTM D445
Molecular Weight 2060 g/molNMR
Vapor Pressure 0.000400 torr
@Temperature 38.0 °C
Knudsen
 1.50 torr
@Temperature 260 °C
Knudsen
 
Thermal PropertiesOriginal ValueComments
Distillation Temperature 140 - 210 °C
@Pressure 0.0000530 MPa
ASTM D1160
Maximum Service Temperature, Air 149 °C
Minimum Service Temperature, Air -57.0 °C
Pour Point -55.0 °CASTM D97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ801 / 253989

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.