MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sorbothane Polyurethane Damping Material, 70 Durometer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the material is deformed, the friction created at the molecular level is generated into heat. High hysteresis is then formed. The energy is moved perpendicularly away from its original plane and is pushed close to 90° out of phase from its original disturbing force.

Sorbothane is used in shock/vibration mounts, stud mounts, and grommets/bushings in diverse fields such as electronics/audio equipment, noise abatement, insoles, protective sports gear, and anti-vibration gloves and wraps.

Information provided by Sorbothane Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 70
Tensile Strength, Ultimate 1.07 MPa500 mm/min; ASTM D412 80
Tensile Stress at Strain 0.490 MPa
@Strain 100 %
ASTM D412 80
Elongation at Break 300 %500 mm/min; ASTM D412 80
100% Modulus 58.0 psi
@Strain 100 %
ASTM D 412-06a
200% Modulus 113 psi
@Strain 200 %
ASTM D 412-06a
300% Modulus 156 psi
@Strain 300 %
ASTM D 412-06a
Compressive Yield Strength 1.31 MPa50% strain; ASTM D575 Method A
 30.0 psi
@Strain 20 %
ASTM D 575-91, Method A
Resilience 15Lupke rebound test
Rebound 25 %Resilience Rebound Height. ASTM D 2632-92. Modified for the effects of tackiness
Bulk Modulus 4.30 GPa
Coefficient of Friction 2.5on polished steel; ASTM D1894
Coefficient of Friction, Static 4.1on polished steel; ASTM D1894
Tear Strength Test 29psi per ASTM 624 with 1 mm nick
Compression Set 4.5 %
@Temperature 22.8 °C,
Time 259000 sec
25% compression; ASTM D395
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 13.1 kV/mmBS 903
 
Thermal PropertiesOriginal ValueComments
CTE, linear 132 µm/m-°C
@Temperature -50.0 - 100 °C
Thermal Conductivity 0.390 W/m-K
Maximum Service Temperature, Air <= 82.0 °COptimum performance range
Minimum Service Temperature, Air >= -29.0 °Coptimum performance range
Glass Transition Temp, Tg -40.0 °C
Flammability, UL94 V-2
 
Descriptive Properties
Bacterial ResistanceNo GrowthASTM G 22
Fungal ResistanceNo GrowthASTM G 21-09
Heat AgingStable72 hours at 158°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sorbothane Polyurethane Damping Material, 50 Durometer
Sorbothane Polyurethane Damping Material, 30 Durometer
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced

PSORB2 / 68440

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.