MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GF 4750 High Density Polyethylene (HDPE), Blow Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes:

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183-1
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 1.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Ball Indentation Hardness 44.0 MPaISO 2039-1
Tensile Strength, Yield 23.0 MPaISO 527-1,-2
Elongation at Yield 10 %ISO 527-1,-2
Tensile Modulus 1000 MPaISO 527-1,-2
Charpy Impact, Notched 5.50 kJ/m²
@Temperature -30.0 °C
Type 1, Edgewise, Notch A; ISO 179
 12.0 kJ/m²
@Temperature 23.0 °C
Type 1, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 70.0 °CB50; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
FNCT (hrs)65ISO 16770, 6.0 MPa, 2% Arkopal N100, 50°C
Processing Methodextrusion blow molding, injection blow molding, injection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake HM 5030 High Density Polyethylene
Ineos T60-3000 HDPE, Narrow MW Distribution
ExxonMobil HMA 018 High Density Polyethylene Resin
Entec Hypel® PEHD30/.950 HDPE
Dow HDPE 30460M High Density Polyethylene

PEQT8485 / 220120

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.