An improved low temperature molten salt bath mixture that will rapidly strip all types of paint. The low temperature allows reclaim of scrap parts that can be immediately repainted without further surface preparation. Durastrip 1500 contains more active ingredients and smokes less than conventional products. Information provided by Heatbath Corporation - Park Metallurgical. Heatbath/Park has been acquired by DuBois Chemicals. |