MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and glass. Offers excellent balance of adhesion onto the substrates and interlayer adhesion with coextruded LDPE and EVA’s.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Cable Shielding
  • Coextrusion Coating
  • Cosmetic Packaging
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Hygiene Packaging
  • Lami Tubes
  • Liquid Packaging

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.933 g/ccExxonMobil method
Acrylic Acid Content 7.5 %ExxonMobil Method
Melt Flow 8.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 1.50 in
@Temperature 280 °C
328 ft/min, constant output at 35 rpm; ExxonMobil Method
 2.00 in
@Temperature 280 °C
164 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 2.83 m/s
@Temperature 280 °C
Constant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 210 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Escor™ 5200 Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5050 ExCo Ethylene Acrylic Acid Copolymer Resin

PEX99130 / 175366

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.