MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo STYRON™ 414 HIPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Availability: Latin America; North America

Features: Food Contact Acceptable; High Flow; High Impact Resistance; High Toughness

Uses: Masterbatch

Agency Ratings: FDA 21 CFR 177.1640

UL File Number: E326906

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cmISO 294-4
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 89ASTM D785
Tensile Strength at Break 2320 psiASTM D638
Tensile Strength, Yield 2760 psiASTM D638
Elongation at Break 70 %ASTM D638
Tensile Modulus 218000 psiASTM D638
Flexural Strength 3480 psiASTM D790
Flexural Modulus 206000 psiASTM D790
Izod Impact, Notched 1.80 ft-lb/inCompression Molded; ASTM D256
 2.20 ft-lb/inInjection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 181 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °FUnannealed; ASTM D648
Vicat Softening Point 205 °FASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 204 - 221 °FZone 6
Rear Barrel Temperature 424 - 480 °F
Middle Barrel Temperature 424 - 480 °F
Front Barrel Temperature 390 - 415 °F
Nozzle Temperature 415 - 469 °F
Zone 1 351 - 379 °F
Zone 2 360 - 399 °F
Zone 3 370 - 410 °F
Zone 4 390 - 421 °F
Zone 5 399 - 430 °F
Adapter Temperature 379 - 450 °F
Die Temperature 390 - 450 °F
Melt Temperature 379 - 450 °FExtrusion
Mold Temperature 60.0 - 150 °F
Back Pressure 29.0 - 174 psi
Cushion 0.250 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1543 / 312236

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.