Product Description: Features: Low flow; Low water carry over during the extrusion process; Good mechanical strength and properties; Suitable for molding of thick walled general purpose articles. Applications: Extrusion: Fine Silt film tape for woven and packaging fabric, e.g. heavy duty bags or flexible intermediate bulk containers (FIBC’s); Packaging strapping; Flat sheet for use in thermoforming applications; Monofilaments for use in ropes, twines, nets and bristles; Coarse silt film tape for ropes and twines. Injection molding: Domestic, industrial and general purpose articles. Blow molding: Moldings up to 1 liter in capacity. Availability: Asia Pacific, Europe, Latin America, North America Additive: Processing Stabilizer Features: Good Processing Stability; Good Strength; Homopolymer; Low Flow; Low Water Carryover Uses: Film; General Purpose; Heavy-duty Bags; Household Goods; Industrial Applications; Monofilaments; Sheet; Strapping; Thick-walled Parts Forms: Pellet Processing Method: Blow Molding; Extrusion; Film Extrusion; Injection Molding; Sheet ExtrusionInformation provided by Sasol Polymers |