MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C18610, TM02 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Mill-hardened Temper, TM - 1/2 Hard

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed

Typical Uses: Connectors, automotive; Connector, appliance, Connector, chemical processing sensor

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 76.0 ksi
Tensile Strength, Yield 70.0 ksi0.5% Ext
Elongation at Break 11 %
Tensile Modulus 18500 ksi
Modulus of Rigidity 7000 ksi
Poissons Ratio 0.30
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000250 ohm-cm70% IACS
Magnetic Permeability 0.999
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 162 BTU-in/hr-ft²-°F
Melting Point 1960 - 1995 °F
Solidus 1960 °F
Liquidus 1995 °F
Annealing Point 660 - 1740 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1700 °F
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.10 - 1.0 %
Cobalt, Co 0.25 - 0.80 %
Copper, Cu 97 - 99.6 %As Balance
Iron, Fe <= 0.10 %
Nickel, Ni <= 0.25 %
Titanium, Ti 0.050 - 0.50 %
Zirconium, Zr 0.050 - 0.40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC18610x1 / 291653

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.