MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Goodfellow Dural® Aluminum /Copper/Magnesium Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: High strength, low weight alloy; in the solution heat-treated and aged condition, mechanical properties are as good as, or better than, low-carbon steel. Limited weldability. Used in aircraft and aerospace applications. Poor corrosion resistance.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 115 - 135
Tensile Strength at Break 420 - 500 MPa
Elongation at Break <= 22 %
Tensile Modulus 73.0 GPa
Izod Impact, Unnotched 0.0800 - 0.220 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000500 ohm-cmTemperature Coefficient of 0.0022 to 0.0026/K
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.5 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 147 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 95 %
Copper, Cu 4.0 %
Magnesium, Mg 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Dural 202/3 CLEAR 0003 Full Rigid Polyvinyl Chloride Compound
Aluminum 2011-T8
Goodfellow Aluminum-Copper/SiC Metal Matrix Composite
AlphaGary Dural 205JB CLEAR 0003 Full Rigid Polyvinyl Chloride Compound
AlphaGary Dural 725C CLEAR 0003 Full Rigid Polyvinyl Chloride Compound

NGOODF144 / 16217

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.