BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging, lamination films, stationary films, and monoaxial oriented films.Information provided by Borealis AG |