MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chase Electronic Coatings HumiSeal® 1A33NS Urethane Conformal Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: HumiSeal® 1A33NS conformal coating is: urethane chemistry, toluene free, chemically resistant, single component, contains no free isocyanates, RoHS Directive 2011/65/EC compliant, Recognized under UL File Number E105698. HumiSeal 1A33NS conformal coating has: excellent moisture and environmental protection for printed circuit assemblies, fluorescence under UV light for ease of inspection.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D1475
Solids Content 44 %± 2. By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 521 g/l
Viscosity 160 - 200 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 75.0 micronsRecommended coating
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 0.0272 GPaDMA
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.60e+10 ohmMoisture; MIL-I-46058C
 2.00e+14 ohmMIL-I-46058C
Dielectric Constant 3.6
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150-98
Dielectric Breakdown 7500 VASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
CTE, linear 193 µm/m-°CTMA
Glass Transition Temp, Tg 26.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Cure Time 0.333 hour
@Temperature 88.0 °C
Option
 0.500 hour
@Temperature 76.0 °C
Option
 720 hour
@Temperature 23.0 °C
Option
Shelf Life 24.0 Month
@Temperature 23.0 °C
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesASTM G21
Thermal Shock-65 to 125°Cper MIL_I_46058C, 50 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAS914 / 239775

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.