Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS). Processing: Injection and compression molding Primary application: Contact bridges, Relays, Circuit breakers (RCD/MCB), Induction Motor connections Information provided by the Raschig Group |