MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexBond™ EA9686.09 K Epoxy Film
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexBond™ EA9686 is a 120°C/250°F cure film adhesive designed for metal, composite and honeycomb bonding applications. Its formulation based on epoxy resin provides a structural resistance over a large temperature range with a good toughness.

Features:

  • Good peel strength
  • Cure from 110°C/230°F to 135°C/275°F (the adhesive can withstand cure up to 177°C/350°F)
  • Storage life: 1 year at or below -18°C/0°F + 4 weeks at room temperature (= 23°C/73°F)
  • Low volatile content (< 1%)
Applications:
  • Metal-to-metal bonding
  • Sandwich construction
  • Composite-to-composite bonding

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 25.0 MPa
@Temperature 120 °C
Lap Shear; EN 2243-1
 30.0 MPa
@Temperature 100 °C
Lap Shear; EN 2243-1
 42.0 MPa
@Temperature 22.8 °C
Lap Shear; EN 2243-1
Peel Strength 46.0 pli
@Temperature 23.0 °C
IGC 04.26.360B
 47.0 pli
@Temperature 100 °C
IGC 04.26.360B
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 89.0 °CWet, 1.5h at 135°C
 89.0 °CWet, 5h at 110°C
 125 °CAs received, 1.5h at 135°C
 129 °CAs received, 5h at 110°C
 
Descriptive Properties
ColorPink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9269 / 322425

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.