MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Perkadox BC-A50 Dicumyl peroxide 50% in aromatic solvent
Categories: Other Engineering Material

Material Notes: Monofunctional peroxide used for crosslinking of natural and synthetic rubbers as well as thermoplastic polyolefins.

CAS number: 80-43-3

EINECS/ELINCS No.: 201-279-3

Applications: Perkadox BC-A50 is used for the crosslinking of natural and synthetic rubbers, as well as thermoplastic polyolefins. Rubber compounds containing Perkadox BC-A50 have good processing safety with a moderate rate of cure. Safe processing temperature (rheometer ts2 > 20 minutes): 130°C. Typical crosslink temperature (rheometer t90 about 12 minutes): 170°C. Data were determined by means of a rheometer in an EPDM-based test compound.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 270.4 g/mol
Storage Temperature <= 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 90.0 °CSelf-Accelerating Decomposition Temperature
Flash Point 46.0 °Cclosed cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.514 - 1.517
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear liquid
Assay49.0-51.0 %
Color<25 APHA
Content (%)5.92Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY798 / 286321

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.