Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this resin exhibit very good strength properties and low seal initiation temperatures.Application/Uses- Agricultural tubing
- Blown film
- Co-ex films
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520.All information provided by Westlake Chemical |
Very good strength properties and low seal initiation temperatures |