Physical Properties | Original Value | Comments |
---|
Density | 0.900 - 1.92 g/cc |
Filler Content | 17.0 - 25.0 % |
Water Absorption | 0.000 - 0.600 % |
Moisture Absorption at Equilibrium | 0.0100 - 0.500 % |
Water Absorption at Saturation | 0.0900 - 0.500 % |
Viscosity | 1.60 - 600000 cP |
| 7.00 - 87.0 cP @Temperature 250 - 285 °C |
| 7.00 - 87.0 cP @Load 1.20 - 5.00 kg |
| 8000 - 800000 cP @Shear Rate 1.00 - 100000 1/s |
| 8000 - 800000 cP @Temperature 230 - 270 °C |
Viscosity Test | 66.5 - 160 cm³/g |
Viscosity Number | 0.600 - 180 cm³/g |
Maximum Moisture Content | 0.0200 |
| 0.200 - 0.200 @Temperature 120 - 120 °C |
| 0.200 - 0.200 @Time 299 - 299 sec |
Linear Mold Shrinkage | 0.00100 - 0.0400 cm/cm |
| 0.00400 - 0.0150 cm/cm @Temperature 80.0 - 80.0 °C |
| 0.0180 - 0.0180 cm/cm @Temperature 260 - 260 °C |
| 0.0180 - 0.0180 cm/cm @Pressure 60.0 - 60.0 MPa |
Linear Mold Shrinkage, Transverse | 0.00160 - 0.0400 cm/cm |
| 0.00900 - 0.0170 cm/cm @Temperature 80.0 - 80.0 °C |
| 0.0180 - 0.0180 cm/cm @Temperature 260 - 260 °C |
| 0.0180 - 0.0180 cm/cm @Pressure 60.0 - 60.0 MPa |
Melt Flow | 3.00 - 570 g/10 min |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Rockwell M | 55.0 - 90.0 |
Hardness, Rockwell R | 107 - 120 |
Hardness, Shore D | 40.0 - 87.0 |
Ball Indentation Hardness | 50.0 - 160 MPa |
Tensile Strength, Ultimate | 26.0 - 178 MPa |
Tensile Strength, Yield | 21.0 - 166 MPa |
| 22.0 - 105 MPa @Temperature -40.0 - 100 °C |
Elongation at Break | 0.600 - 300 % |
| >= 100 % @Temperature 60.0 - 120 °C |
Elongation at Yield | 1.00 - 75.0 % |
Modulus of Elasticity | 0.420 - 23.4 GPa |
| 0.180 - 0.900 GPa @Temperature 60.0 - 120 °C |
Flexural Yield Strength | 22.0 - 275 MPa |
| 14.0 - 127 MPa @Temperature 60.0 - 150 °C |
Flexural Modulus | 0.231 - 18.1 GPa |
| 0.500 - 5.80 GPa @Temperature 60.0 - 150 °C |
Flexural Strain at Break | 2.00 - 6.00 % |
| 4.60 - 7.00 % @Temperature 60.0 - 150 °C |
Flexural Strain at Yield | 5.00 - 8.90 % |
Adhesive Bond Strength | 31.0 - 42.0 MPa |
Izod Impact | 5.00 - 186 J |
| 30.0 - 144 J @Temperature -30.0 - -20.0 °C |
Izod Impact, Notched | 0.0400 - 8.00 J/cm |
| 0.300 - 0.300 J/cm @Temperature -20.0 - -20.0 °C |
| 1.30 - 5.70 J/cm @Temperature -40.0 - -20.0 °C |
| 1.30 - 5.70 J/cm @Thickness 1.57 - 3.18 mm |
Izod Impact, Unnotched | 0.374 - 5340 J/cm |
| 5.25 - 6.00 J/cm @Temperature -30.0 - -30.0 °C |
Izod Impact, Notched (ISO) | 1.98 - 170 kJ/m² |
| 2.00 - 20.0 kJ/m² @Temperature -40.0 - -20.0 °C |
Izod Impact, Unnotched (ISO) | 4.20 kJ/m² - NB |
| 3.80 kJ/m² - NB @Temperature -40.0 - -30.0 °C |
Charpy Impact Unnotched | 0.294 J/cm² - NB |
| 2.50 J/cm² - NB @Temperature -40.0 - -20.0 °C |
Charpy Impact, Notched | 0.120 - 1000 J/cm² |
| 0.200 - 2.50 J/cm² @Temperature -40.0 - -20.0 °C |
Gardner Impact | 0.904 - 40.0 J |
Tensile Impact Strength | 65.0 - 160 kJ/m² |
Dart Drop, Total Energy | 2.00 - 140 J |
Puncture Energy | 15.0 - 16.0 J @Temperature -30.0 - -30.0 °C |
Coefficient of Friction | 0.130 - 0.660 |
Coefficient of Friction, Static | 0.130 - 0.730 |
Tensile Creep Modulus, 1 hour | 1500 - 2400 MPa |
Tensile Creep Modulus, 1000 hours | 950 - 11000 MPa |
K (wear) Factor | 4.03 - 423 x 10-8 mm³/N-M |
|
Electrical Properties | Original Value | Comments |
---|
Electrical Resistivity | 1000 - 1.20e+17 ohm-cm |
Surface Resistance | 10.0 - 2.00e+17 ohm |
Dielectric Constant | 2.90 - 4.20 |
Dielectric Strength | 14.0 - 140 kV/mm |
Dissipation Factor | 0.00100 - 0.0330 |
Arc Resistance | 60.0 - 240 sec |
Comparative Tracking Index | 120 - 600 V |
Hot Wire Ignition, HWI | 7.00 - 120 sec |
High Amp Arc Ignition, HAI | 15.0 - 120 arcs |
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 25.4 mm/min |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 12.0 - 170 µm/m-°C |
| 25.2 - 171 µm/m-°C @Temperature 22.8 - 150 °C |
CTE, linear, Transverse to Flow | 36.0 - 150 µm/m-°C |
| 90.0 - 170 µm/m-°C @Temperature 22.8 - 150 °C |
Specific Heat Capacity | 1.50 - 1.97 J/g-°C |
Thermal Conductivity | 0.131 - 0.330 W/m-K |
Melting Point | 200 - 271 °C |
Maximum Service Temperature, Air | 90.0 - 200 °C |
Hot Ball Pressure Test | 125 - 200 °C |
Deflection Temperature at 0.46 MPa (66 psi) | 55.0 - 387 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 216 °C |
Deflection Temperature at 8.0 MPa | 45.0 - 48.0 °C |
Vicat Softening Point | 65.0 - 221 °C |
Glass Transition Temp, Tg | 60.0 °C |
UL RTI, Electrical | 75.0 - 150 °C |
UL RTI, Mechanical with Impact | 75.0 - 140 °C |
UL RTI, Mechanical without Impact | 75.0 - 150 °C |
Flammability, UL94 | HB - 5VA |
Oxygen Index | 20.0 - 32.0 % |
Glow Wire Test | 650 - 960 °C |
|
Optical Properties | Original Value | Comments |
---|
Transmission, Visible | 0.600 - 90.0 % |
|
Processing Properties | Original Value | Comments |
---|
Processing Temperature | 20.0 - 300 °C |
Nozzle Temperature | 225 - 295 °C |
Adapter Temperature | 225 - 275 °C |
Die Temperature | 215 - 275 °C |
Melt Temperature | 174 - 295 °C |
Mold Temperature | 10.0 - 160 °C |
Drying Temperature | 80.0 - 150 °C |
Moisture Content | 0.000 - 0.250 % |
Dew Point | -28.9 °C |
Injection Pressure | 3.45 - 120 MPa |
Vent Depth | 0.00127 - 0.00381 cm |
Precipitation Temperature | 40.0 - 270 °C |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.