MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Guarniflon PFA Perfluoroalkoxy Polymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for applications up to 260°C. Thanks to its fluidity during the processing, the final products in PFA - especially the skived film - are absolutely porous-free, hence very suitable for electrical applications.

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.12 - 2.17 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55 - 60ASTM D2240
Tensile Strength >= 30.0 MPaASTM D638
Elongation at Break >= 380 %ASTM D638
Flexural Modulus 600 MPaASTM D790
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 30.0 - 40.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 - 200 µm/m-°C
@Temperature 23.0 - 100 °C
ASTM D696
Thermal Conductivity 0.240 W/m-KASTM D177
Melting Point 300 - 310 °C
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® PFA Fluoropolymer Film
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
Lucite International Colacryl® DP300 Specialty Acrylic Resin
Isoflon PFA Polyperfluoroalkoxyethylene
Henkel Loctite® 290 Wicking Grade Threadlocker

PGUARN020 / 142753

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.