MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical Zinc Stearate (Zn-st)
Categories: Other Engineering Material

Material Notes: Advantages:
  • Non-toxic stabilizer
  • With no sulfur pollution
  • Good lubricity
  • Prevent from initial dyeing
  • Enhance a product’s waterproof ability
Applications:
  • Applied to non-toxic PVC products processing
  • Used as additives for polymer products manufacturing (PP, PE, PS, EPS)
  • Used as mold release agents for rubber products manufacturing
  • Used as extenders for sanding sealer for wood products
  • For food flexible packaging bags
  • Used as water-proofing agents for asbestos floor tiles
  • Used as lubricant

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc10kg
 1.15 g/cc15kg
 1.30 g/cc20kg
Particle Mesh Size 325 Meshpass >98%
 
Thermal PropertiesOriginal ValueComments
Melting Point 115 - 125 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn >= 10 %
 
Descriptive Properties
AppearanceWhite powder
Composition<1%Free fatty acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN895 / 267203

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.