(Viewing data as-entered.
Click here
to return)
Intercontinental Polymers CoPET 198 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polyethylene Terephthalate (PET)
;
Polyethylene Terephthalate (PET), Unreinforced
Material Notes:
Applications: Low Melt
Information provided by Intercontinental Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Viscosity Measurement
0.55 - 0.61
Intrinsic; LCL-PR21
Optical Properties
Original Value
Comments
Transmission, Visible
90 %
clear; thickness not quantified
Gardner Color Number
-3.00 - 3.0
+ b; LCL-PR01
23 - 43
Rd; LCL-PR01
Processing Properties
Original Value
Comments
Melt Temperature
190
°C
LCL-PR29
Moisture Content
<= 0.25 %
LCL-PR08
Descriptive Properties
DEG
1.7 - 2.3 wt%
LCL-PR11
Isophthalic Acid
24 - 26 mol%
LCL-PR42
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Intercontinental Polymers CoPET 159 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Intercontinental Polymers CoPET 120 CoPET Polymer Type 159 - Clear, Low Melt Polyester Pellets
Intercontinental Polymers CoPET 214-02 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Intercontinental Polymers HoPET 728-02 Clear, Polyester Pellets
PINTER20 / 48204
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.