CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensional accuracy. Applications: Mechanical, electric and electronic components that need stiffness and strengthMechanical, electric and electronic components that need extremely high dimensional accuracy.Mechanical, electric and electronic components that need electric conductivity or antistatic propertyInformation provided by Teijin Chemicals Ltd. |