MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Arlon Electronic Materials 99ML Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Thermally conductive laminate and prepreg circuit board material

Information provided by ARLON Electronic Materials.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Peel Strength 5.00 pli1 oz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°Cx,y direction
CTE, linear, Transverse to Flow 44.0 µm/m-°Cz direction
Thermal Conductivity 1.00 W/m-K
Glass Transition Temp, Tg 175 °C
Decomposition Temperature 291 °COnset
 303 °C5 percent
Flammability, UL94 V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)5
IPC Delamination - T288 (minutes)0
IPC Delamination - T300 (minutes)0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arlon Electronic Materials 91ML Low-Cost Halogen-Free Thermally Conductive Epoxy
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
Aremco Aremco-Bond™ 525 Electrically & Thermally Conductive Material, Silver Filled
Armstrong A-12 Epoxy Adhesive, at 1:1 Mix Ratio
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive

PARLM9858 / 149011

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.