MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODAFAC® RS-410 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: Phosphate Esters, Branched Alcohol Ethoxylate based

CAS: 9046-01-9

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAFAC RS-410 very effective APE Free primary anionic surfactants for acrylic, styrene acrylic and vinyl acrylic latex syntheses.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 100 - 115KOH to First INFL. PT.; RP-0427
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.80 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Cloudy LiquidRP-0064
CompositionNonionic Content<11%, RP-0351
Critical Micelle Concentration (%)0.002
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RS-610 Surfactant
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAFAC® RA-600 Surfactant
Solvay RHODAFAC® PA15 Surfactant
Solvay RHODAFAC® PA23 Surfactant

WRHOD368 / 137599

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.