MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M CS-195+ Composite Sheet
Categories: Other Engineering Material

Material Notes: 3M Fire Barrier CS-195+ Composite Sheet is one-part composite system comprised for four components. The heart of the system is an organic/inorganic, fire-resistive elastomeric sheet. It is bonded on one side to a layer of 28 gauge galvanized steel. The other side is reinforced with hexagonal shaped steel-wire mesh and covered with aluminum foil. This material is designed to seal larger penetrations through fire-rated walls and floors. It is also used for shielding cable trays and conduit, HVAC ductwork and vital process equipment from radiant heat, flame spread and smoke. It functions as an effective intermittent fire-break within horizontal and vertical cable try runs, and is excellent for both new and retrofit construction. The nominal 7.62 mm thick composite sheet provides up to a 4-hour fire rating. IT is lightweight and can be easily installed with common trade tools. When exposed to temperatures in excess of 121°C, the fire-resistive sheet begins to volumetrically expand and swells 8-10 times its original size, forming a high strength, hard char that retards heat transmission. This expansion process is called “intumescence.” Under normal operating conditions this material is a good thermal conductor which allows unwanted heat build-up to escape from process and control equipment and also minimizes power cable derating.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45 - 65Non-flame supporting hardness
Tensile Strength at Break 0.645 MPaASTM D412, Method A
Elongation at Break 489 %ASTM D412, Method A
Compression Set <= 25 %
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 119 kV/inASTM D149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A227 Steel Wire, Class I
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1010 Steel, cold drawn
Sandvik 75X1 Spring Wire

PMM35450 / 170197

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.