MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions XV3871 Vinyl Compound - Flexible (FPVC)  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Description/Features:

  • Transparent
  • High Flow
  • Does not contain di (ethyl hexyl) phthalate
  • Gamma Resistant

Applications:

  • FDA (Medical)
  • Hose and Tubing

Processing Method:

  • Extrusion

Disclaimer: NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is “For foods of high water content only”. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9510 sec; ASTM D2240
Tensile Strength, Ultimate 2784 psiType 4 - Flexibles, 20 in/min, 100% in/in; ASTM D638
 3570 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 316 %Type 4 - Flexibles, 20 in/min; ASTM D638
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aurora Plastics GA-7056D-FR-105 PVC
EMS-Grivory Grilamid® TR XE 4139 black 9231 PA*
INEOS Styrolution Luran® HD-20 SAN
Ineos Nova 3100 General Purpose Crystal Polystyrene
Geon® Performance Solutions 87614 Molding PVC

PH1PO2468 / 44566

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.