This low density polyethylene is tailored for cast film applications that require: - Excellent openability
- Suited for high speed converting
- Good clarity
- Low COF
Typical cast film applications include: - Bakery film
- General purpose packaging
Information provided by Chevron Phillips. Formerly branded with the MarFlex® trade name. |