MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 92015 Double Coated Tape with Adhesive 200MP
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provides exceptional temperature and chemical resistance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.70 milFaceside Adhesive
 2.70 milBackside Adhesive
 4.20 milCaliper
 5.00 milCarrier
 5.90 milTotal Thickness
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 1.25 pliPP, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 1.5625 pliPP, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 3.75 pliABS, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 4.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 4.6875 pliPC, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
 5.00 pliABS, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 5.9375 pliPC, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 9.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1300 kV/in
Dielectric Breakdown 7600 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CLong term
 149 °CShort term
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type200MP
LinerTan, 58# Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain CHR® 2253-2 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive
Permabond TA430 Acrylic Adhesive & Initiator
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive

PMM33271 / 168018

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.