MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FRPC10 Flame Retardant for PC
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Go Yen Chemical Industrial Co., Ltd. (GYC Group) has developed a flame retardant that is especially for the PC industry - GY-FR-PC10. It has high thermal stability and is compatible with various PC products. With only small amounts, GY-FR-PC10 can successfully increase the value of a product. In this manner, GY-FR-PC10 has now become a specified flame retardant to many of the PC manufacturers.

Intro: PC are a group of thermoplastic polymers with good properties that find many applications. The needs for PC are gradually growing in construction industry, automobile industry, electronics industry, and so forth. However, PC is combustible; as a result, the needs for flame retardant for this material are becoming popular. Go Yen Chemical Industrial Co., Ltd. (GYC Group) has developed a flame retardant that is especially for the PC industry - GY-FR-PC10. It has high thermal stability and is compatible with various PC products. With only small amounts, GY-FR-PC10 can successfully increase the value of a product. In this manner, GY-FR-PC10 has now become a specified flame retardant to many of the PC manufacturers.

Advantages:

  • Provide excellent flame-retardant effect and impact resistance to the product
  • With good heat tolerance and thermal stability
  • Will not cause migration after added
  • Increase the value of a product with only adding small amounts of the additive
  • With only little influence to the PC properties
Applications:
  • Any kinds of PC products
  • Outer skin of vehicles and scooters
  • Automotive parts
  • PC signboard, construction board
  • Smartphone case, computer case, TV shell
  • Lampshade, light tube, lens, bullet-proof glass
  • Sport bottle, milk bottle

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 6.5 - 7.0
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 300 °C
 
Descriptive Properties
AppearancePowder
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN033 / 266341

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.