MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 7335Z Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Random Copolymer with Anti-stat Additives

Applications: Housewares, storage boxes, pill vials and containers.

Formolene 7335Z is a high flow random copolymer containing anti-stat. It also contains a unique combination of stabilizers that give it excellent processing, impact and usage performance. Its clarity makes it an excellent choice for "see-through" rigid packaging including housewares.

Specimens were injection molded according to the conditions specified in ASTM D4101.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 35 g/10 min
@Temperature 230 °C
I2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 4000 psi2" (50mm) per min.; ASTM D638
Elongation at Yield 11 %2" (50mm) per min.; ASTM D638
Flexural Modulus, 1% Secant 150000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 1.50 ft-lb/inASTM D256
 1.7 ft-lb/inASTM D256

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound
AKG Polymers Vision PP PPC BL1010 T20 Polypropylene Compound
Formosa Plastics Formolene® 3335N Random Copolymer Polypropylene
Formosa Plastics Formolene® 3335E Random Copolymer Polypropylene
Ineos R35C-00 Polypropylene Random Copolymer

PFPCPP58 / 38914

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.