MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 525 Electrically & Thermally Conductive Material, Silver Filled  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Electrically Conductive, Silver-Filled, One-Part Epoxy Paste.
Good Chemical Resistance and Mechanical Strength to 340 ºF.

Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 g/cc
@Temperature 25.0 °C
mixed
Particle Size <= 28 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76
Shear Strength 2500 psiTensile Shear
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.01 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.90 W/m-K
Maximum Service Temperature, Air 340 °Fcontinuous
 375 °Fintermittent
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 149 °C
Recommended Cure
 6.00 hour
@Temperature 121 °C
Alternative Cure
Shelf Life 6.00 Month
 
Descriptive Properties
ColorSilver
FillerSilver Flake
Mixed ViscosityPaste

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
Abatron AboWeld 8505-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
AdvanSix Capran® 526 Heat-Stabilized Nylon Film, Blown Tubular Film
Aptek THERM-PAD 1100 Thermally conductive silicone pad

ZPAREM16 / 24280

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.