MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® LP27 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® LP27 Isocyanate is a special modified pure 4,4'-diphenylmethane diisocyanate that is a clear liquid at 27°C. Unlike pure 4,4'-MDI, Lupranate® LP27 Isocyanate has enhanced storage stability as a liquid at moderate temperatures. With a functionality of 2.01 and very high 4,4'-MDI content, Lupranate® LP27 can be used in place of pure 4,4'-MDI in many applications, including the preparation of prepolymers, elastomers, sealants and adhesives.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Viscosity 17 cP
Vapor Pressure 1.33e-8 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
Flash Point 200 °C
 
Descriptive Properties
ColorPale Yellow
CompositionNCO content0.324

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Lupranate® LP30 Isocyanate
BASF Lupranate® 281 Isocyanate
BASF Lupranate® 5010 Isocyanate
BASF Lupranate® 8020 Isocyanate
BASF Lupranate® 81 Isocyanate

PBASG0687 / 132320

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.