Emerson & Cuming 9 Eccobond® General Purpose Catalyst General purpose, low viscosity. Imparts good physical strength and chemical resistance to cured castings. Recommended for most general purpose applications. Cure Type: Room Temp or Heat The Eccobond® product line is now a part of Henkel; this specific grade is discontinued. |