MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2275B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2200 series is a general purpose thermoplastic elastomer series, available in BLK, designed for exterior automotive molding applications. Sarlink ME-2275B is a medium hardness, low density, UV stabilized grade suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Low Density; Medium Hardness; Low Specific Gravity; Light Stabilized; Low Flow; Lubricated; Sunlight Resistant; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccISO 1183
Viscosity 203 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 72
@Time 15.0 sec
Injection Molded; ISO 868
 74
@Time 5.00 sec
Injection Molded; ISO 868
 77
@Time 1.00 sec
Injection Molded; ISO 868
 72.9
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 74.2
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 74.6
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 75.5
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 77.3
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 78.8
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 1020 psiFlow, Type 1, 20 in/min; ISO 37
 1650 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1030 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 1060 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 1710 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 1720 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 360 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 473 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 383 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 168 hr; ISO 188
 391 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 534 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 534 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 650 %Flow, Type 1, 20 in/min; ISO 37
 840 %Across Flow, Type 1, 20 in/min; ISO 37
 638 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 672 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 841 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 843 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 180 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 210 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 42 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 64 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 86 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 400 - 420 °F
Front Barrel Temperature 410 - 430 °F
Nozzle Temperature 420 - 440 °F
Melt Temperature 420 - 440 °F
Mold Temperature 60.0 - 90.0 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1065 / 237556

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.