MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Arquad 268-75
Categories: Other Engineering Material

Material Notes: Arquad 268-75 is vegetable based di(C16-C18 alkyl) dimethyl ammonium chloride.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.849 g/cc
@Temperature 63.0 °C
 0.854 g/cc
@Temperature 54.0 °C
 0.859 g/cc
@Temperature 46.0 °C
 0.882 g/cc
@Temperature 25.0 °C
pH 6.0 - 8.0
Viscosity 50 cP
@Temperature 66.0 °C
 55 cP
@Temperature 60.0 °C
Vapor Pressure 0.0586619 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 80.0 °C
@Pressure 0.101325 MPa
Initial
Pour Point 40.0 °C
Flash Point 25.0 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.00 - 2.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 8.0 - 10 %
 
Descriptive Properties
AppearancePaste
Content= 0.15 %Sulphated ash
 = 1.5 %Free Amine & Amine Salt
 74 - 76 %Active content
Equivalent mass576 g/eq
HLB3Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY294 / 285817

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.