MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Picco™ A140 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Picco™ A140 Hydrocarbon Resin is a low molecular weight, amber colored thermoplastic resin produced from petroleum-derived monomers. Picco™ A140 is characterized by its excellent resistance to acids, alkalies and moisture. It shows good color stability and, when formulated with elastomers, a good balance of flex, tear, tack and adhesion properties. This resin is particularly indicated as processing and reinforcing agent in rubber compounds and as binder in protective coatings. Picco™ A140 Hydrocarbon Resin is polymerized under conditions that control its softening point within a narrow range.

Application/Uses:

  • Building and Construction
  • Contact Adhesives
  • Graphic Arts
  • Hot Melt Adhesives
  • Lithographic and letterpress oil-based inks
  • Paint and Coatings
  • Solventborne Adhesives
  • Varnish
Key Attributes:
  • Excellent pigment wetting
  • Excellent resistance to acids, alkalis and moisture
  • Excellent water repellant
  • Non-reactive
  • Thermoplastic

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
Viscosity 15000 cP50% in Halterman Test Oil 6/9
Molecular Weight 940 g/molMn
 1800 g/molMw. Mw/Mn ratio = 1.9
 3300 g/molMz
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 140 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 6.0ASTM D6166

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5530 / 222724

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.