MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChevronTexaco ISO 150 Marine Oil E
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines.

The base ouils are compounded to emulsify readily with water and to form a rich creamy emulsion which lubricates the crosshead bearings, crankshaft bearings, and guides. Historically, whale oil was used as the emulsifying agent. Since whale oil is no longer available, synthetic rape speed oil is used.

Chevron Marine Oils E are designed to meet the critical demands of plain bearing and pump piston rod lubrication in a wet environment. To achieve this, the oil is formulated to use the moisture or steam condensate from the cylinders as a part of the lubricant. This is accomplished by using an emulsifying agent in the oil which mixes with the moisture, forming a rich creamy emulsion. This lathering action resists the washing effect of the saturated steam and lubricates the bearings and guides in reciprocating engines.

Applications

Chevron Marine Oils E ISO 150 and 220 differ mainly in the amount of emulsifying agent used. Chevron Marine Oil E ISO 150 and 10% emulsifying agent an Chevron Marine Oil E ISO 220 has 15%.

These oils can feed readily through wicks or a drop feed oiler. In other cases, they are poured from an oil can into a “pot” on the crosshead or crankshaft bearing where condensate condenses down from the steam cylinder above, emulsifies with the oil, and lubricates the bearings.

Chevron Marine Engine Oils E can be used as marine stern tube lubricants where oils complying with MIL-L-15019E Symbols 4065 an 6135 are required. MIL-L-15019E specifies emulsifying type lubricants. Do not use Chevron Marin Oils E where the OEM requires a nonemulsifying oil, as is the case with some types of stern tubes.

Chevron Marine Oils E can be used for the lubrication of air tools where excessive moisture is present and where a medium viscosity oil, similar in compounding to steam cylinder oil, is required.

Chevron Marine Oils E are authorized by USDA for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.

Key Words: CPS Number: 235403; MSDS Number: 6957
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 21.1 °
Viscosity Measurement 69Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 759 SUS
Saybolt Viscosity at 210°F 69 SUS
Kinematic Viscosity at 40°C (104°F) 143 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 12.3 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -27.0 °CASTM D97
Flash Point 188 °CASTM D92
 
Descriptive Properties
Emulsifying Agent, %10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV081 / 74696

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.