MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUMIPLAS LD8550 Light diffusion ABS, Injection & Extrusion grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Light diffusion, Weatherability

Application: (LED) Lamp cover, Signboard, Lighting decoration of electronic device

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 630 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Strength 93.2 MPa
@Thickness 6.40 mm
15mm/min; ASTM D790
Flexural Modulus 23000 kg(f)/cm²
@Thickness 6.40 mm
15mm/min; ASTM D790
Izod Impact, Notched 80.0 kg-cm/cm
@Thickness 3.20 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 120 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.500 mm
 V-2
@Thickness 1.60 mm
 V-2
@Thickness 2.50 mm
 V-2
@Thickness 3.00 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 57 %
@Thickness 1.00 mm
JIS K7361
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 270 °CInjection Molding
Middle Barrel Temperature 280 - 300 °CInjection Molding
Front Barrel Temperature 290 - 310 °CInjection Molding
Nozzle Temperature 290 - 310 °CInjection Molding
Zone 1 260 - 280 °CExtrusion Molding
Zone 2 270 - 300 °CExtrusion Molding
Zone 3 270 - 300 °CExtrusion Molding
Zone 4 270 - 300 °CExtrusion Molding
Adapter Temperature 280 - 300 °CExtrusion Molding
Die Temperature 260 - 295 °CExtrusion Molding
Melt Temperature 290 - 310 °C
Mold Temperature 80.0 - 120 °CInjection Molding
Roll Temperature 120 - 150 °CBottom, Extrusion Molding
 120 - 150 °CMiddle, Extrusion Molding
 120 - 150 °CTop, Extrusion Molding
Drying Temperature 100 - 120 °C
@Time 10800 - 18000 sec
Moisture Content <= 0.020 %
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding
 
Descriptive Properties
Outdoor Suitabilityf1UL746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9800 / 239316

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.