MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound MF004AS Polypropylene, Unspecified (PP, Unspecified)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP THERMOCOMP MF004AS compound is based on Polypropylene (PP) resin containing 20% glass fiber. Added features of this grade include: Heat Stabilized.

Features: High Stiffness,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
 1.034 g/ccASTM D792
Moisture Absorption 0.0300 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm24hrs; ASTM D955
 0.0072 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0090 - 0.010 cm/cm24hrs; ASTM D955
 0.0095 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPaASTM D638
 65.0 MPaISO 527
Elongation at Break 2.2 %ISO 527
 2.3 %ASTM D638
Tensile Modulus 4550 MPa50 mm/min; ASTM D638
 5100 MPa1 mm/min; ISO 527
Flexural Strength 92.0 MPaASTM D790
 104 MPaISO 178
Flexural Modulus 4340 MPaASTM D790
 5600 MPaISO 178
Izod Impact Notched 48.0 JASTM D256
Izod Impact, Unnotched 325 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 Jpeak; ASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=0.750 mm
UL 746A
 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.750 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 74.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 145 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 149 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.750 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 240 - 250 °C
Melt Temperature 225 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81714 / 289661

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.