MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik POLYVEST® EP-OC 1200 S Polybutadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: POLYVEST EP-OC 1200 S is a maleic anhydride adduct of a low molecular weight cis-1.4-polybutadiene. This polybutadiene adduct has succinic anhydride groups randomly distributed along the polymer chains. This makes the originally apolar polybutadiene more polar and thus accessible for various chemical reactions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/cc
@Temperature 20.0 °C
DIN 51 757
Iodine Absorption Number 380 - 420g of Iod/ 100g; DIN 53 241
Viscosity 61000 cP
@Temperature 20.0 °C
DIN EN ISO 3219
Molecular Weight 2500 g/molGPC
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 130DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Pour Point -1.00 °CDIN ISO 3016
Flash Point >= 300 °CDIN EN ISO 2719
Ignition Temperature 355 °CDIN 51 794
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.5DIN ISO 4630

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Buna® cis 132 High-cis polybutadiene rubber (nickel catalyzed) for tires and rubber articles
Evonik POLYVEST® 110 Liquid
ATG s.r.l. BR Polybutadiene Rubber
Fujipoly Industries Sarcon® NR-HTc Gap Filler Pad
LG Chemical BR 1208 Polybutadiene Polymer

PHUMB341 / 81343

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.