MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M BBI-A Shrinkable Tubing for Bus Bar
Categories: Polymer; Thermoset

Material Notes: 3M Heat Shrinkable Tubing for Bus Bar BBI-A Series is designed for insulating rectangular, square and round bus bar rated from 5 kV through 35 kV. It will also cover and insulate inline bolted connections of rectangular bus bars. The tubing meets the requirements of ANSI/IEEE Standard C37.20. The standard tubing lengths are 20 ft (6.1 m) and 50 feet (15.2m). 3M BBI-A Tubing is made of a specially formulated cross-linked polyolefin. The tubing is colored orange-red. The material has high resistance to splitting, good solvent resistance to splitting, good solvent resistance and excellent tracking resistance properties. The tubing shrinks easily with industry standard methods, forming an aesthetically appealing insulation cover.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.30 %7 days at RT; MIL-I-23053/15A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5.60 - 16.5 MPaFluid Resistance, 24 hrs immersed; MIL-I-23053/15A
 15.0 MPaASTM D257
 10.0 MPa
@Treatment Temp. 175 °C,
Time 605000 sec
Accelerated Aging; MIL-I-23053/15A
Elongation at Break 575 %ASTM D638
 400 %
@Treatment Temp. 175 °C,
Time 605000 sec
Accelerated Aging; MIL-I-23053/15A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 287 - 451 kV/inFluid Resistance, 24 hrs immersed; MIL-I-23053/15A
 550 kV/in
@Thickness 1.78 mm
ASTM D149
Track Resistance 25200 sec1 in @ 2.5 kV; ASTM D2303

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35208 / 169955

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.