MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Film 0F016 PMMA
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: PLEXIGLAS® Film 0F016 is a high weather resistant, glossy and transparent acrylic film for graphic printings and high quality laminations. Due to its excellent performance under weathering and UV light exposure, PLEXIGLAS® Film 0F016 does not present color change or yellowing. Therefore it provides high protection of laminating systems from degradation caused by UV radiation. Its glossy and very smooth surface leads the film to have an excellent optical quality surface.

Application: PLEXIGLAS® Film 0F016 can be used to be printed on as high quality film decoration and then laminated on different polymeric films and sheets. Laminated decoration films based on PLEXIGLAS® are suitable for a wide range of molding processes such as thermoforming, and insert molding. In labels and tapes, PLEXIGLAS® Film 0F016 can be used as single face layer or clear overlay in laminate systems for high UV and weathering protection. High gloss and quality finishing is achieved. Due to its good optical property and lamination with pressure sensitive adhesive (PSA), PLEXIGLAS® Film 0F016 is recommended for traffic control signs under long term outdoor application. Due to its very good optical properties, PLEXIGLAS® Film 0F016 can be used as overlay in high quality ID Cards.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccDIN 53479
Surface Tension 50 dynes/cmDIN 53364
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 47.0 MPaISO 527-3
Elongation at Break >= 25 %ISO 527-3
Elongation at Yield 6.0 %ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 101 °CISO 11357
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489
Transmission, Visible >= 92 %ISO 13458-2
UV Transmittance <= 1.0 %
@Wavelength 280 - 380 nm
DIN EN 410

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V825 Acrylic
Trinseo Plexiglas® SG7 Acrylic
Trinseo Plexiglas® HT121 Acrylic
Röhm Plexiglas® zk6BR Molding Compound
Röhm PLEXIGLAS® XT Clear 0A070 UV transmitting PMMA

PEVONIL029 / 196234

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.