MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinoid 1345 Phenolic Molding, Glass Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Data provided by the manufacturer.

Resinoid 1345 is a glass reinforced, two-step phenolic molding compound. It was specifically developed for molded electric motor commutators where performance for prolonged periods at elevated temperatures while under centrifugal loads is critical. This material comes in pelletized from and is suitable for injection, transfer or compression molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccASTM D792A
Water Absorption 0.10 %24 hours R.T.; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cmPositive Mold; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110ASTM D785
Tensile Strength, Ultimate 59.0 MPaASTM D651
Flexural Strength 83.0 MPaASTM D790
Flexural Modulus 15.0 GPaASTM D790
Compressive Strength 186 MPaASTM D695
Izod Impact, Notched 1.30 ft-lb/inASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 11.8 kV/mmShort Time; Dry; ASTM D149
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 300 °CASTM D648
Flammability, UL94 V-0
 
Descriptive Properties
COLORBLACK
FORMPELLET

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPHR02B / 253977

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.