MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRILOY™ Compound D2000 Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRILOY D2000 compound is based on Polycarbonate (PC) resin containing a proprietary non-halogenated lubrication system. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
 1.17 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.140 %23°C/50% RH/24 hrs; ASTM D570
 0.180 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm24hrs; ASTM D955
 0.0070 - 0.0090 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm24hrs; ASTM D955
 0.0070 - 0.0090 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPaISO 527
 60.0 MPaASTM D638
Tensile Strength, Yield 51.0 MPaISO 527
 53.0 MPaASTM D638
Elongation at Break 98.6 %ISO 527
 125.6 %ASTM D638
Elongation at Yield 5.6 %ISO 527
 6.5 %ASTM D638
Tensile Modulus 1860 MPa50 mm/min; ASTM D638
 2120 MPa1 mm/min; ISO 527
Flexural Strength 78.0 MPaISO 178
 82.0 MPaASTM D790
Flexural Modulus 2130 MPaASTM D790
 2130 MPaISO 178
Izod Impact Notched 704 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 58.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 137 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 40.0 Jpeak; ASTM D3763
Impact Test 45.0 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.16ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.090ASTM D3702 Modified: Manual
K (wear) Factor 60.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 74.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 73.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 73.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 142 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 130 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 280 - 300 °C
Zone 3 280 - 310 °C
Melt Temperature 290 - 315 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 100 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81126 / 289073

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.