MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccResin Density
 1.75 g/ccFiber Density
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 550 MPaRT; Dry; EN2561
 650 MPa90º, RT, Dry; EN2561
 600 MPa
@Temperature 75.0 °C
90º, Wet; EN2561
 600 MPa
@Temperature 100 °C
90º, Wet; EN2561
 650 MPa
@Temperature 75.0 °C
Wet; EN2561
 700 MPa
@Temperature 100 °C
Wet; EN2561
Tensile Modulus 57.0 GPa90º, RT, Dry; EN2561
 65.0 GPaRT; Dry; EN2561
 60.0 GPa
@Temperature 75.0 °C
90º, Wet; EN2561
 62.0 GPa
@Temperature 100 °C
Wet; EN2561
 63.0 GPa
@Temperature 100 °C
90º, Wet; EN2561
 66.0 GPa
@Temperature 75.0 °C
Wet; EN2561
Compressive Yield Strength 650 MPaRT; Dry; DIN65380
 730 MPa90º, RT, Dry; DIN65380
 415 MPa
@Temperature 100 °C
Wet; DIN65380
 435 MPa
@Temperature 100 °C
90º, Wet; DIN65380
 495 MPa
@Temperature 75.0 °C
90º, Wet; DIN65380
 500 MPa
@Temperature 75.0 °C
Wet; DIN65380
Compressive Modulus 57.0 GPaRT; Dry; DIN65380
 61.0 GPa90º, RT, Dry; DIN65380
 50.0 GPa
@Temperature 100 °C
90º, Wet; DIN65380
 52.0 GPa
@Temperature 100 °C
Wet; DIN65380
 53.0 GPa
@Temperature 75.0 °C
Wet; DIN65380
 60.0 GPa
@Temperature 75.0 °C
90º, Wet; DIN65380
Shear Strength 60.0 MPa0º, ILSS (Short Beam), RT, Dry; EN2563
 75.0 MPaIn-Plane, RT, Dry; EN6031
 35.0 MPa
@Temperature 100 °C
0º, ILSS (Short Beam), Wet; EN2563
 42.0 MPa
@Temperature 75.0 °C
0º, ILSS (Short Beam), Wet; EN2563
 58.0 MPa
@Temperature 100 °C
In-Plane, Wet; EN6031
 68.0 MPa
@Temperature 75.0 °C
In-Plane, Wet; EN6031
 
Processing PropertiesOriginal ValueComments
Shelf Life 14.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Cured Thickness per Ply (cm)0.38
Fiber Volume (%)50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Hexcel® HexPly® F593 Epoxy Resin, W3T282 Carbon Fabric
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric

PHEXC156 / 98626

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.