MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Outokumpu 725LN Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes:

Applications: Wet corrosion resistance and general service.

Available in hot rolled plate (Quarto) form.

Key Words: EN 1.4466; UNS S31050
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 630 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 250 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 290 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 320 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 135 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 160 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 195 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 55 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 200 GPaRT
 170 GPa
@Temperature 400 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature 100 °C
 17.0 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.440 J/g-°CRT
Thermal Conductivity 12.0 W/m-KRT
 17.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 25 %
Iron, Fe 50.65 %
Molybdenum, Mo 2.2 %
Nickel, Ni 22 %
Nitrogen, N 0.13 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 904L High Performance Austenitic Stainless Steel
Outokumpu SAF 2507® Duplex Stainless Steel
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Outokumpu 304 PRODEC® Stainless Steel
Outokumpu 316 PRODEC® Stainless Steel

NOUTOK31 / 18746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.