MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Tosoh Ethylenedichloride
Categories: Other Engineering Material

Material Notes: Applications:
  • Agricultural Chemicals
  • Chelating Agents
  • Corrosion Inhibitors
  • Ethylene Urea Resins
  • Ion Exchange Resins
  • Lubricants for Thermoplastic Resin
  • Oil Additives
  • Polyamide Resins
  • Reforming Agents for Soils
  • Rubber Chemicals
  • Surface-active Agents
IMCO No.: 8

UN No.: 1604

CAS No.: 107-15-3

Information provided by Tosh Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.897 - 0.910 g/cc
Molecular Weight 60.1 g/mol
Vapor Pressure 9.00 torr
 
Thermal PropertiesOriginal ValueComments
Melting Point 8.00 °C
Boiling Point 22.0 °C
@Pressure 0.00133 MPa
 49.0 °C
@Pressure 0.00667 MPa
 116 °C
@Pressure 0.101 MPa
Distillation Temperature >= 115 °CInitial Boiling Point
 <= 119 °CDry Point
Flash Point 41.5 °CCOC
 
Descriptive Properties
AppearanceClear and free of suspended matters
Color<15APHA
Purity>99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOSOH102 / 306557

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.