MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ FC 2260 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Fluoroelastomer FC 2260 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2260 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.
  • Composition: di-polymer of vinylidene fluoride and hexafluoropropylene plus cure site monomer
  • Can be used in blends with fluorosilicone, silicone, EDPM and other peroxide curable elastomers
  • Process targets: transfer and compression molding and calendering
  • Peroxide cure technology
  • Slightly improved water and steam resistance over conventional fluoroelastomer
  • Vulcanization of thick cross-section parts without fissuring

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Mooney Viscosity 60
@Temperature 121 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 2345 psiPress Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 225 %Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.745 ksi
@Strain 100 %
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 25 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature -18.0 °CTR10; ASTM D1329
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 65.9 %
 
Descriptive Properties
ColorTranslucent to Off-White
MH, Maximum Torque11.1 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque2.1 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
SolubilityPartially soluble in low molecular weight esters and ketones
t`50, Time to 50% cure1.1 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure3 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min0.8 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ FLS 2650 Fluoroelastomer
Momentive Performance Materials FSE7340 Heat Cured Fluorosilicone Rubber
A. Schulman Alcryn® 2180 BK Melt Processable Rubber
Rogers Arlon R37503G015 0.015" (0.381 mm) Cured Fluorosilicone Rubber
Wacker Elastosil® LR 6240 A/B Liquid Silicone Rubber

PDYNE117 / 34925

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.